Mada za sehemu hiiPreparing preservative solutionsMada 4
- Handling preservative chemical
- Determining wood volume
- Performing treatment
- Determining retention and penetration of preservative
When wood is treated with preservatives, two important factors determine how well the wood will be protected: retention and penetration. Retention tells us how much preservative stays in the wood, while penetration tells us how deeply the preservative enters the wood. Both must be measured correctly to ensure treated wood lasts long and resists decay, insects, and fungal attacks.
What is Retention?
Retention is the amount of preservative chemical that remains in the wood after treatment. It is measured in kilograms of preservative per cubic meter of wood (kg/m³). This is important because wood needs enough preservative to be toxic to wood-destroying organisms. If retention is too low, the wood will not be properly protected and will decay quickly.
Why Retention Matters
- Adequate retention ensures the wood remains protected throughout its service life
- Different uses require different retention levels (above ground, ground contact, or marine use)
- Insufficient retention leads to premature failure of the wood
Gravimetric Method (Weight Loss Method)
The gravimetric method is the most widely used technique for determining retention. It involves measuring the weight of wood before and after treatment.
Steps for the gravimetric method:
- Weigh the wood before treatment – Measure the clean, dry wood sample and record its initial weight (W₁)
- Treat the wood – Apply preservative using pressure impregnation, dipping, or spraying
- Weigh the wood after treatment – Measure the weight after treatment and drying (W₂)
- Calculate retention – Use the formula:
\text{Retention} \left( \frac{\text{kg}}{\text{m}^3 \right) = \frac{\text{Weight of preservative retained (kg)}}{\text{Wood volume (m}^3\text{)}}
The weight of preservative retained equals: W₂ - W₁
Worked Example 2.4: Calculating Retention
Given data:
- Initial weight of untreated wood (W₁) = 50 g
- Weight of treated wood after drying (W₂) = 60 g
- Volume of wood sample (V_wood) = 100 cm³
Solution:
Step 1: Calculate the mass of preservative retained
Mass retained=W2−W1=60 g−50 g=10 g
Step 2: Convert to kilograms
10 g=0.01 kg
Step 3: Convert wood volume to cubic meters
100 cm3=100×10−6 m3=0.0001 m3
Step 4: Calculate retention
Retention=0.0001 m30.01 kg=100 kg/m3
Alternatively, using the simpler form:
Retention=100 cm310 g=0.1 g/cm3=100 kg/m3
Answer: The retention of preservative in the wood is 100 kg/m³
When measuring retention, consider these factors to ensure accurate results:
- Wood species – Porous woods like pine retain more preservatives than dense woods like oak
- Moisture content – Dry wood absorbs more preservative; high moisture hinders absorption
- Preservative type – Water-based, oil-based, or solvent-based preservatives behave differently
- Treatment method – Pressure treatments achieve higher retention than non-pressure methods
- Concentration of solution – Stronger solutions generally lead to higher retention
- Wood density – Dense wood may resist penetration, reducing retention
- Post-treatment drying – Improper drying or exposure to rain can cause leaching, reducing retention
What is Penetration?
Penetration refers to how deeply the preservative chemical enters the wood, measured from the surface toward the core. Effective penetration ensures that the preservative reaches all vulnerable parts, especially the sapwood, which is most susceptible to decay and insect attack.
Why Penetration Matters
- Without adequate penetration, only the outer layers are protected while the interior remains vulnerable
- Full sapwood penetration is essential for proper protection
- Penetration requirements vary by wood use – for example, TANESCO specification (S11) for utility poles requires minimum sapwood penetration of 20 mm at the ground line
Using an Increment Borer
An increment borer is a specialized tool used to extract wood cores from treated poles or timber.
Steps to test penetration:
- Select a treated pole or sawn timber sample
- Use an increment borer to extract a core from the wood
- Measure the depth of penetration in millimeters from the surface toward the core
- If the penetration boundary is unclear, apply chrome azurol (CCA indicator) – this chemical reagent colours the penetrated area clearly
The penetrated zone must meet the minimum depth requirements specified by standards.
- Wood species – Softwoods (like pine) allow better penetration due to lower density; hardwoods have denser structures
- Moisture content – Wood should have about 30% moisture content for optimal uptake; too dry or too wet wood delays absorption
- Preservative type – Oil-based preservatives penetrate deeper than water-based ones
- Treatment process – Pressure treatment (full-cell and empty-cell) ensures deep penetration; non-pressure methods (brushing, dipping) result in shallow penetration
Several international standards guide acceptable levels:
| Standard | Purpose |
|---|---|
| AWPA U1 | Defines minimum retention and penetration levels for various preservatives |
| AWPA C14 | Provides methods for determining retention |
| EN 351-1 | Guidelines on durability and retention based on wood's intended use |
| EN 351-2 | Methods for assessing penetration depth and retention |
| ISO 9087 | Determines effectiveness by measuring penetration |
| ISO 3348 | Methods for determining retention per unit volume |
In Tanzania, the Tanzania Bureau of Standards (TBS) aligns with these international standards to ensure wood preservation quality.
In Tanzania, carpenters and builders use retention and penetration measurements when treating timber for construction of houses, furniture, and utility poles. For example, when treating pine poles for fencing at a construction site in Arusha, a carpenter must ensure the preservative penetrates at least 20 mm into the sapwood and retains at least 4 kg/m³ of CCA to protect the fence posts from termite attack and fungal decay. This ensures the fence lasts many years even during the rainy season, saving money on frequent replacements.
Jinsi utakavyotathminiwaTathmini ya mchakato · Tathmini ya matokeo · Tathmini ya maarifa
Tathmini ya mchakato
- Select tools for determining retention and penetration of preservative
- Determine retention of preservative
- Determine penetration of preservative
- Observe safety
- Clean tools
- Store tools
Tathmini ya matokeo
Retention and penetration of preservatives in wood well determined as per standards
Tathmini ya maarifa
Knowledge evidence:
Detailed knowledge of:
Method used: The students should explain how to:
- Select proper tools for determining retention and penetration of preservative in wood
- Determine retention and penetration
Principles: Determining retention and penetration of preservative
Theories: The student should explain procedures for retention and penetration
Detailed knowledge about: Safety precautions involved in retention and penetration of preservatives
Swali
What is meant by the term retention in wood preservation?
Ingia ili kuwasilisha jibu lako na lihesabiwe katika umahiri wako.
Ingia ili kufanya mazoeziMwalimu
Umekwama? Niulize chochote kuhusu mada hii.
Ingia ili kumuuliza Mwalimu wa AI wa Sonza kuhusu swali hili.
Ingia ili kuulizaMajadiliano
Hakuna maswali bado